Nickel Superalloy Bolts are essential fasteners in applications that combine high operational temperatures, high mechanical stress, and aggressive corrosive media. Alloys like Inconel and Hastelloy are primarily nickel-based, formulated with chromium, molybdenum, and other elements to maintain exceptional strength, creep resistance, and oxidation resistance, even above 540°C (1000°F). These high temperature bolts are vital in power generation, jet engine assembly, and petrochemical processing. Zeron Fasteners is a trusted manufacturer and supplier in India, providing a full range of these sophisticated corrosion resistant fasteners to meet stringent industry specifications.

Related Products

Nickel Superalloy Bolt 333

Nickel Superalloy Bolts Chemical Composition

Element Composition
Nickel (Ni) 50.0 - 55.0
Chromium (Cr) 17.0 - 21.0
Iron (Fe) Balance
Niobium (Nb) 4.75 - 5.50
Molybdenum (Mo) 2.80 - 3.30
Titanium (Ti) 0.65 - 1.15
Aluminum (Al) 0.20 - 0.80
Cobalt (Co) 1.0 max

Nickel Superalloy Bolts Mechanical Properties

Property Value (Aged Condition)
Tensile Strength, minimum 1240 MPa min
Yield Strength, minimum 1035 MPa min
Elongation 12% min
Maximum Service Temperature 700°C
Creep Rupture Strength Excellent